A buyer-focused guide to PEEK, small-hole and precision-plastic deburring with the OLLITAL T6
Quick answer: dry ice blasting can be a strong deburring option when the burr is small, accessible to a directed nozzle and located on a precision plastic or machined component where loose abrasive media, water or aggressive hand tools are undesirable. The process is especially interesting for through holes, blind holes, cross-holes, fine edges and recessed geometry because dry ice sublimates after impact rather than remaining inside the part as blasting grit. It is not a universal replacement for mechanical deburring or cryogenic batch finishing, so representative sample testing should be part of the purchasing process.
This is a different buying problem from general industrial cleaning. The acceptance criteria may include complete burr removal, preservation of a polished or dimensional surface, access to a 2 mm hole, no loose media left in a cavity, repeatable cycle time and enough throughput to support the machining or molding line. Searches such as dry ice deburring machine, PEEK deburring, plastic deburring machine, burr removal from small holes, micro deburring and precision-parts dry ice cleaning therefore need a more specific answer than a general dry ice blasting guide.
Deburring normally refers to unwanted material left by machining, drilling, milling, trimming or another subtractive process. Deflashing usually describes thin excess material created at a mold parting line, gate or other molding feature. Cleaning removes contamination such as oil, particles, residues or process films without intentionally removing part material. The distinction matters because the burr or flash itself becomes the material that must be separated.
A flexible whisker on the edge of a machined PEEK hole can behave very differently from a thick structural burr. A thin molded flash can behave differently from an internal machining burr hidden at the intersection of two holes. Before choosing equipment, define which defect is actually present.
A 2026 open-access study in the International Journal of Advanced Manufacturing Technology provides useful context: early CO2-based cleaning patents targeted removal of flash and burrs from thermoplastic and elastic materials, while later CO2 snow work expanded into precision particle and film contamination removal. That history explains why CO2-based processes sit at the boundary between cleaning and finishing.
Precision plastic parts are often small but geometrically demanding. Engineering polymers may be selected for dimensional stability, chemical resistance, low weight, electrical properties or other functional reasons. Those benefits can be compromised if post-processing scratches a sealing surface, rounds a critical edge, changes a thread or leaves abrasive particles inside a small passage.
Machining creates burrs where tools exit holes, intersect internal passages or leave thin material along edges. On a simple component, an operator may remove the burr with a knife, brush or rotary tool. On a part with many 2–5 mm holes, blind cavities or cross-holes, manual access becomes slow and results can vary between operators.
PEEK is a high-performance engineering thermoplastic, but the material name alone is not enough to select a deburring process. Grade, fillers, wall thickness, machining conditions, burr root strength and acceptance requirements all matter. The quotation request should describe where the burr is, how large it is, how deeply the feature is recessed and which dimensions or surfaces must remain unchanged.
Linde’s current cryogenic deflashing and deburring guidance lists CO2 snow as a method for deburring and deflashing plastic parts and includes PEEK among thermoplastics used in cryogenic finishing applications. This supports the process category, but every PEEK part still needs application-specific validation.

The strongest candidates are usually fine burrs in accessible holes, recesses and complex features where targeted nozzle access is possible and loose secondary blasting media is undesirable.
Through holes are relatively straightforward to inspect because both sides may be visible. The trial should record hole diameter, wall thickness, burr root strength, nozzle alignment and the inspection standard after processing. If many identical holes are present, the supplier should also demonstrate a repeatable sequence rather than cleaning one convenient feature.
Blind holes are more demanding because the burr is recessed and the feature limits nozzle access. A dry ice stream can be attractive because the blasting medium sublimates instead of leaving solid grit behind, but the nozzle still needs a practical angle and enough working distance to deliver useful energy to the burr root.
Cross-holes create an internal edge at the intersection of two passages. A brush or knife may not reach the burr consistently, while a targeted dry ice jet can sometimes access the feature through one of the passages. The sample trial should show that the burr is actually removed, not merely polished or bent out of sight.
Specialist provider Nitrofreeze describes dry ice deburring as useful for hard-to-reach burrs in blind and through holes and recessed geometry, while also emphasizing that burr formation, location and intensity determine which finishing process is appropriate.
Fine burrs around threads, grooves and external edges can also be candidates when the defect is small enough to remove without over-processing the surrounding part. These features become especially interesting when manual brushing creates inconsistent results or when loose abrasive media would be difficult to remove afterward.
Dry ice blasting is not a universal solution. Thick, ductile or structural burrs may be too strongly attached for the required cycle time. A burr that behaves like part of the geometry may require cutting, machining, abrasive finishing or another dedicated process. Very deep features can also be difficult when the nozzle cannot direct enough energy to the defect.
A failed sample test is still valuable because it prevents the buyer from purchasing the wrong machine. It can also reveal that dry ice is useful only for selected holes or finishing steps rather than the entire part.
No single finishing method wins every application. The best choice depends on burr location, access, batch size, repeatability, media requirements and the surface that must be preserved.
Hand tools, brushes, knives and rotary tools are flexible and familiar. They can be excellent for low-volume parts, thick burrs and locations where the operator can see and reach the defect directly. The limitations appear when features become very small or repetitive: labor time rises, results depend more heavily on operator technique and internal access becomes difficult.
Cryogenic batch deburring freezes unwanted material so it becomes more brittle, then uses tumbling and/or process media to remove it. This can be effective for large batches of molded or machined parts with suitable geometry. The limitation is not that batch processes are inferior; it is that the geometry must allow the process media to reach the defect. Extremely small or recessed features may require a targeted alternative.
Dry ice blasting is a targeted process. The operator or automated system aims a nozzle at the defect and controls the air, dry ice feed, angle, distance and dwell time. Its practical advantage for precision parts is that the dry ice medium sublimates after impact, so conventional blasting grit is not left inside the part. The trade-off is that every feature still needs line-of-nozzle access and the cycle must be fast enough for production.
OLLITAL’s current T6 PCB Precision Components Dry Ice Blasting Machine is positioned for precision components, small gaps and complex surfaces where controlled dry ice delivery is more important than broad heavy-duty cleaning.
| Current Published Item | T6 Reference | Buyer Interpretation |
|---|---|---|
| Dimensions | 640 × 400 × 580 mm | Compact format for precision work areas |
| Equipment weight | 55 kg | Workshop-portable, but not handheld |
| Headline blast pressure | 4.0–6.0 bar | Confirm working condition for the actual nozzle and part |
| Air consumption | 0.8–4.0 m³/min (28–141 CFM) | Compressor sizing should use delivered airflow |
| Air supply pressure | 0.1–0.8 MPa listed in parameter table | Page also lists a 4–6 bar blast-pressure headline; confirm current configuration |
| Dry ice delivery | 0–0.55 kg/min adjustable | Useful for low-media precision trials |
| Hopper capacity | Maximum 10 kg | Supports longer testing or production runs |
| Protection level | IP52 | Check against installation environment |
OLLITAL states that current product parameters may be updated, so the published values should be treated as reference data. Precision deburring should be quoted around the nozzle, part geometry and validated process rather than a single headline pressure number.
OLLITAL reports in a November 2025 factory-test case involving a Malaysian customer that the customer brought a PEEK application involving burrs on small machined parts and small holes. According to the company’s published case report, the T6 demonstration addressed 2 mm holes and the customer proceeded with an order after the test.
The important lesson is not that every 2 mm hole is guaranteed to work. Hole depth, burr shape, material grade, orientation, nozzle access and inspection standard can change the result. The case shows that a small-hole PEEK deburring project is realistic enough to justify a controlled sample test.
Precision deburring does not need maximum pressure by default. It needs stable and repeatable conditions. If the compressor is undersized, pressure can fall during the trial and make the process look inconsistent. If the air contains excessive moisture or contamination, valves, hoses and repeatability can also suffer.
Provide the supplier with available pressure, continuous airflow, air-dryer information, hose length and whether other equipment shares the same compressor. Compressor sizing should be based on delivered airflow at the required pressure, not only motor horsepower or the compressor’s maximum pressure rating.
In micro-deburring, the nozzle is part of the process design. It determines whether the dry ice stream reaches the burr root, how concentrated the jet is, how much air the setup consumes and whether the operator can keep a repeatable working distance. A long nozzle may help with a recessed feature but interfere with a fixture or camera. A smaller nozzle may improve precision but demand a different air condition.
For this reason, send drawings and close-up photos instead of only describing the material. The supplier can evaluate the actual approach angle and propose a more realistic gun and nozzle combination.

A controlled sample test should document the starting burr, geometry, protected surfaces, process settings, final inspection and production cycle.
Measure or photograph the burr before testing. Record where it was created, approximate thickness and height, whether it is flexible or brittle, and whether it is connected along a long edge or only at a small root. The defect must be defined well enough that the buyer can judge whether the trial truly removed it.
Provide hole diameter, depth, cross-hole position, edge location and working clearance. If the part contains dozens of identical holes, show the complete pattern so the supplier can estimate a practical production path rather than demonstrate only the easiest feature.
A precision finishing process needs both a removal target and a protection target. Record critical dimensions, sealing surfaces, polished areas, threads, coatings, roughness or cosmetic requirements that must remain within tolerance.
Begin with conservative parameters and change one variable at a time where practical: air pressure, dry ice feed, nozzle type, stand-off distance and dwell. The objective is not to find the most aggressive setting; it is to find a repeatable process window that removes the burr with minimum unnecessary energy and media.
Use the same inspection method that production will use. For micro-holes, that may include a microscope, borescope or magnified visual inspection. Critical parts may also require dimensional verification before and after processing.
A successful one-part demonstration is only the first gate. Record active blasting time, loading and unloading, dry ice consumption, compressor demand, inspection time and the number of parts that can be completed per hour. The production decision should use the full cycle, not only trigger-on time.
• Machine model: Exact machine and configuration used in the trial.
• Nozzle: Nozzle type, outlet geometry and any extension.
• Air conditions: Working pressure and approximate continuous airflow.
• Dry ice setting: Media feed setting and relevant dry ice preparation.
• Working distance: Approximate stand-off distance and angle.
• Cycle time: Active blasting plus practical handling time per part or batch.
• Result documentation: Before/after images and inspection method.
• Surface condition: Dimensional, roughness or cosmetic observations relevant to acceptance.

Typical T6 dry ice deburring workflow for molded and machined precision plastic parts.
A successful hand-held test does not automatically define the production method. A low-volume shop may prefer manual operation because part mix changes frequently. A higher-volume plant may need a fixture that holds the part at a repeatable angle and allows the same hole pattern to be processed in a fixed sequence.
Automation becomes attractive when part geometry and burr location repeat consistently. The engineering job is to reproduce the validated process window: nozzle position, distance, travel speed, air condition and media feed.
A 2026 study on automated CO2 snow cleaning for precision optical mould tools is relevant to this production question because it evaluates replacing manual cleaning with a controlled automated CO2 process for delicate tooling. The application is not identical to T6 deburring, but it illustrates why controlled motion and process repeatability matter in precision CO2-based finishing.
A buyer may ask why a precision machine is necessary when a larger industrial dry ice blaster can also propel dry ice. The useful distinction is not simply power. General industrial models are suited to molds, machinery, automotive parts and broad contamination. A precision project may place more importance on low adjustable media feed, fine nozzle options, compact work-area integration and the ability to observe or fixture a small part.
If the project is still at the general equipment-selection stage, start with OLLITAL’s Dry Ice Blasting Machine Selection Guide. If the real problem is micro-burr removal on machined plastic parts, a T6-specific sample trial becomes the more useful next step.
• Part material: PEEK, PTFE, nylon, PPS, acetal, metal or another material; include grade and fillers if known.
• Part drawing: Dimensions, critical tolerances, hole diameters, depths and cross-hole positions.
• Burr description: Machining operation, burr height/thickness, location and whether flash is also present.
• Surface requirement: Cosmetic, polished, sealing or functional areas that must remain unchanged.
• Current process: Hand deburring, brushing, tumbling, cryogenic batch, chemical or another method.
• Volume: Prototype quantity, parts per hour, daily demand and expected scale.
• Compressed air: Available pressure, continuous airflow, dryer/filtration and hose distance.
• Inspection method: Microscope, visual inspection, dimensional gauge, roughness or customer-specific standard.
• Automation target: Manual bench work, fixture-assisted processing or production-cell integration.
• Destination and utilities: Voltage/frequency, installation country and documentation requirements.
It can be suitable for some PEEK burrs, especially fine burrs on small holes, edges and recessed geometry. Suitability depends on burr root, geometry, grade and surface requirement, so representative sample testing is recommended.
OLLITAL reports a T6 customer trial involving PEEK parts and 2 mm holes. This is relevant evidence, but not a universal guarantee because hole depth, burr shape and nozzle access vary.
Dry ice deburring is typically a targeted blasting process using dry ice particles and compressed air. Cryogenic deburring often freezes parts and uses tumbling and/or process media in a batch system.
The dry ice itself sublimates into CO2 gas after impact, so it does not remain as mineral or polymer blasting grit. Removed burr material still needs to be managed and the part should be inspected.
The process is often selected to reduce aggressive mechanical contact, but dimensional stability should still be verified on the actual part. Critical features should be measured before and after sample processing.
Through holes, blind holes, cross-holes and recessed features can be candidates when the nozzle can deliver useful energy to the burr. Very deep or inaccessible geometry may limit the process.
A thick or structural burr may require a mechanical or other dedicated finishing process. Dry ice should be tested rather than assumed to work.
The current T6 page lists air consumption of 0.8–4.0 m³/min and a 0.1–0.8 MPa air-supply range, while the headline specification lists 4.0–6.0 bar blast pressure. Confirm the actual compressor condition for the proposed nozzle and application.
OLLITAL currently lists an adjustable dry ice delivery range of 0–0.55 kg/min and a maximum 10 kg hopper. Precision deburring may use much less than the maximum setting.
Yes. For precision deburring, a representative sample trial is one of the most valuable purchasing steps. Send the real burr condition, drawings and acceptance criteria so settings and cycle time can be documented.
Yes, when the part geometry and burr location repeat consistently. Automation should reproduce a validated process window using controlled nozzle position, distance, speed, air and media feed.
The current product page also positions T6 for precision components in electronics, molds, aerospace, medical equipment and automotive applications. The actual result still needs material-specific validation.
For an independent overview of CO2 snow cleaning in precision manufacturing, see the 2026 Springer / International Journal of Advanced Manufacturing Technology study. For industrial plastics and deburring context, review Linde’s cryogenic deflashing and deburring guidance and Nitrofreeze’s dry ice / cryogenic deburring information. These references help distinguish targeted dry ice blasting from batch cryogenic finishing.
Dry ice deburring is most valuable when it solves a geometry problem, not simply when it replaces a brush. Fine burrs in small holes, cross-holes, blind features and precision plastic components can be difficult to reach consistently with manual tools or loose media. A targeted dry ice process offers a dry finishing route in which the blasting medium sublimates after impact, but the result still depends on burr geometry, nozzle access, compressed air and process settings.
For precision PEEK and small-hole projects, OLLITAL’s T6 Precision Components Dry Ice Blasting Machine is the most relevant current product page to review. The strongest purchasing approach is to send representative parts first, define acceptance criteria and use the test data to decide whether the T6 configuration and cycle are suitable.
Need help evaluating a precision deburring application?
Send part drawings, material, burr photos, hole size, current finishing method, required output and available compressed-air data. OLLITAL can review the application and arrange a sample-oriented evaluation before the final machine configuration is confirmed.